易文辉, 曹猛, 封伟, 韦玮, 吴洪才, 陈烽, 杨文正, 杨青. 一种偶氮接枝聚氨酯材料的光致变色性质[J]. 发光学报, 2002,23(2): 179-182
YI Wen-hui, CAO Meng, FENG Wei, WEI Wei, WU Hong-cai, CHEN Feng, YANG Wen-zheng, YANG Qing. Photoisomerization of ACID Orange2/PU Copolymer[J]. Chinese Journal of Luminescence, 2002,23(2): 179-182
采用接枝共聚的方法合成了一种具有偶氮侧基的聚氨酯材料
利用旋转涂膜法制备了该材料的薄膜。在室温下测试了该薄膜的吸收光谱和光致变色性质。并且研究了曝光时间与激光功率密度对光致变色性质的影响。发现
该材料在波长为532nm激光作用下
500nm处吸收减弱
360nm处吸收增强。随着曝光时间的延长和激光功率密度的增大
这种变化趋势增强。
In the past decade optical recording media has become a subject of extensive scientific and industrial interest. Good stability
high optical sensitivity
high storage densities
and short access time for optical storage are very important. Azobenzene derivatives are typical materials displaying a reversible photoismerization and are of great potential application as optical information storage media and optical switching systems
[1~4]
. The incorporation of photoisomerizable azobenzene molecules in polymer matrix has been the trend of current research in the area of optical information storage materials because of the mutual exploitable characteristic performances
that is
the ease of device fabrication and the photoreponsiveness of azobenzene units
which can trigger property changes as a result of the conformational change of the molecules. In the previous work
novel azo dye grafted polyurethane (HSANB/PU) has been synthesized and characterized. In this study we report the laser-induced photoismerization property of this graft polymer. The UV-vis absorption spectrum of HSANB/PU film is shown in Fig.1
from which we can see that there are two absorption peaks at 320nm and 500nm
which attribute to cis-form and trans form of HSANB/PU respectively. Generally speaking
the absorption peak of trans form azo compound is at 440nm or so
however this peak shifts to nearly 500nm mainly because of the conjugating effect of benzene and naphthalene ring. Therefore Nd:YAG laser with the output wavelength at 532nm is used to induce the photoisomerization of the polymer film because it is in the resonance region. The spectrum of absorption versus time of HSANB/PU irradiated by 532nm laser with power density of 40mW/cm
2
is shown in Fig.2
which shows that absorption at 520nm decreased
while absorption peak at 360nm increased when the sample is irradiated by the given laser
which indicated the trans-cis transition of the azo compound. Moreover the absorption at 520nm decreased steadily and the absorption increased steadily while the irradiation time ranges from 0~15min. The spectrum of absorption versus power density of HSANB/PU irradiated by 532nm laser for 60s is shown in Fig.3
which shows that the absorption at 520nm decreased steadily and the absorption increased steadily while the irradiation power density ranges from 2~40mW. The effect of intensifying irradiation power is equivalent to that of prolonging irradiation time. Moreover the photoisomerization threshold of the material is only 2mW/cm